产品详情
高铝瓷球(瓷柱)主要含量以氧化铝为主,具有足够的化学稳定性和热稳定性。作为反应器内催化剂的支撑、覆盖材料及塔填料,广泛用于化工、化肥、冶炼、天然气、陶瓷等 行业。它具有纯度高、强度好、耐磨、耐高温、耐强酸和强 碱等特点。
化学成份/Chemical Composition
| AI2O3含量/Content成份/Ingredients | 高铝瓷球/High aluminaceramic ball | ||||
| 90% | 93% | 95% | 97% | 99.5% | |
| AI2O3 | ≥90% | ≥93% | ≥95% | ≥97% | ≥99.5% |
| SiO2 | ≤5% | ≤4% | ≤3% | ≤1% | ≤0.2% |
| Fe2O3 | ≤0.5% | ≤0.5% | ≤0.1% | ≤0.1% | ≤0.05% |
| MgO | ≤1% | ≤1% | ≤1% | ≤0.5% | ≤0.05% |
| Na2O+K2O | ≤1% | ≤1% | ≤1% | ≤0.5% | Na2O≤0.2% |
| CaO | ≤1% | ≤1% | ≤1% | ≤0.5% | ≤0.02% |
物理性能/Physical Properties
| ' AI2O3含量/Content物理性能/PhysicalProperties | 高铝瓷球/High aluminaceramic ball | |||||
| 90% | 93% | 95% | 97% | 99.5% | ||
| 耐热温度/Heat ResistanceTemperature℃ | 1450℃ | 1500℃ | 1550℃ | 1600℃ | 1650℃ | |
| 吸水率/Water Absorption % | ≤4% | |||||
| 耐酸度/Acidity Resistance% | ≥98% | |||||
| 耐碱度/Alkali Resistance % | ≥96% | |||||
| 耐温度急变/Resistanttosuddentemperature changes℃ | ≥800℃ | |||||
| 抗压强度/CompressiveStrengthKN/PM | 3 | ≥0.20 | ≥0.25 | ≥0.3 | ≥0.4 | ≥0.5 |
| 6 | ≥0.50 | ≥0.60 | ≥0.8 | ≥1.0 | ≥1.2 | |
| 8 | ≥0.65 | ≥0.8 | ≥1.0 | ≥1.2 | ≥1.6 | |
| 10 | ≥1.0 | ≥1.3 | ≥1.6 | >2.0 | ≥2.4 | |
| 13 | ≥1.8 | ≥2.3 | ≥2.9 | ≥3.6 | ≥4.5 | |
| 16 | ≥2.6 | ≥3.2 | ≥4.0 | ≥5.0 | ≥6.3 | |
| 20 | ≥3.2 | ≥4.0 | ≥5.0 | ≥6.3 | ≥8.0 | |
| 25 | ≥4.0 | ≥5.0 | ≥6.3 | ≥8.0 | ≥10.0 | |
| 30 | ≥4.5 | ≥5.6 | ≥7.0 | ≥9.0 | ≥11.0 | |
| 38 | ≥6.0 | ≥7.5 | ≥9.3 | ≥12.0 | ≥15.0 | |
| 50 | ≥10.0 | ≥12.5 | ≥16.0 | ≥19.5 | ≥24.0 | |
| 60 | ≥12.0 | ≥15.0 | ≥19.0 | ≥23.0 | ≥29.0 | |
| 75 | ≥15.0 | ≥19.0 | ≥23.0 | ≥29.0 | ≥37.0 | |
| 堆积密度/Bulk Density kg/m3 | ≥1.8 | ≥1.8 | ≥1.85 | ≥1.85 | ≥1.9 | |